Why Halogen-free low-smoke flame-retardant cable outsheath cracks ?

2 years ago 5947 0 News

1684289123934604.jpg

The Causes of Cracks in the Outer Sheath of LSZH Flame Retardant Cables


Halogen Free Flame Retardant Cables are a special cable more common and troublesome quality problem is the environmental stress cracking of insulating materials. 


Low smoke and halogen-free are abbreviated as LSZH, LSOH, LS0H, LSFH, and OHLS, which is the material classification of wire sheathing in the wire and cable industry.
Low smoke zero halogen wire sheathing is composed of thermoplastic or thermosetting materials that have low smoke emissions when exposed to heat and do not contain halogens themselves.

It also reduces the amount of toxic, corrosive gases produced when it burns.
Low smoke and halogen-free materials are often used in poorly ventilated environments such as airplanes, train cars, or ships.
It is also commonly used in the railroad industry, where there are high-voltage lines or signal lines that transmit the location of trains underneath the railroad.
The use of halogen-free cable materials also reduces the accumulation of toxic gases when the line is damaged by fire or a short circuit.

Halogen-free low-smoke flame retardant cable materials are caused by environmental stress cracking the main reasons are:

Caused By The Polymer Properties

Due to the high filling of flame retardant filler such as aluminum hydroxide, magnesium hydroxide causes the strength of the polymer body to reduce, elongation and flexibility also reduce, tear-resistance and cracking resistance inherent. 

Halogen-free carriers are generally used low-density polyethylene and EVA, the flame retardant with the mixture of high hardness, in particular, to meet the IEC332-1 flame retardancy (single combustion level, the material.

The corresponding oxygen index is generally greater than and the material hardness at this time is often greater than the shore A90 above.

Material Extrusion Process

Based on the metal hydrate as a flame retardant halogen free cable material, high filling properties.

Such as the extrusion process temperature, and the screw compression ratio used improperly, will cause hydrous oxide decomposition and high Cut the polymer off. 

As the compression ratio, the extruder speed can not reach the normal level, resulting in the material in the barrel and screw residence time being too long, the friction generated by the high temperature, and the hydrous oxide premature decomposition of the material inside the bubble (Micro hole). 

So that the finished product after extrusion mechanical strength and anti-winding ability greatly reduced.

Sudden cooling also adds unfavorable factors.

Factors In The Use Of The Environment And Storage Conditions

Polyethylene-based halogen-free low-smoke materials are generally more temperature-sensitive. 

Under the conditions of large temperature changes, the internal stress due to thermal expansion and contraction tends to cause cracking in the interface area. 

For example, in the north, when a finished cable reel of halogen-free flame retardant cable is placed on the customer's site without packaging, a week later, almost all the cables on the reel were found to have longitudinal cracks on the sunny side of the cable, 1/2 circumference of the disk. 

This analysis is due to the cable tray on one side of the sun, one side of the shade, and both sides of the larger temperature difference under the effect of bending stress and material cracking.

Extrusion Dies

Extrusion dies structure type, stretch ratio, and the balance of tension and extrusion stress after the elimination of internal stress have a crucial role. 

Generally, use less pressure semi-extrusion mold. 

The draw ratio and stretch balance ratio of the inner and outer molds should be controlled at 1: 2 and close to 1 respectively.

The tensile balance rate is calculated as follows:

Where: Dd - Die diameter (mm)

DT - outside diameter of the core (mm)

DCW-- cable insulation or jacket diameter after extrusion (mm)

DBW - core diameter (mm)

@ZMSCABLE SUPPLIER 

Tags:
LSZH Cable
INQUIRY
主站蜘蛛池模板: 爱爱一区| 国产gv在线观看受被做哭 | 青青热久免费精品视频在线播放 | 亚洲成人精品久久 | 美女张开腿让男生桶视频 | 午夜春色 | 日韩精品久久久毛片一区二区 | 校园都市经典激情另类 | 性饥渴少妇XXXXⅩHD | 播放一级黄色片 | 久久国产免费 | 一级毛片手机在线观看 | 九色porny在线观看 | 免费一级特黄录像 | 欧美一区二区在线看 | 欧美二区精品 | 欧美xx视频| 国产乱理伦片在线观看 | 最近2019年中文字幕 | 少妇精品久久 | av狼友永久免费网址观看 | 久久久久久成人 | 在线精品一区二区 | 1区2区免费视频 | 日日干日日 | 樱桃视频高清免费观看在线 | 种付おじさんと在线观看 | 草草影院在线观看 | 在线观看亚洲人 | 久久国产免费观看精品3 | 亚洲视频在线观看免费视频 | 免费播放毛片 | 囯产丰满肉体A片 | 欧美成人v | AAAA级少妇高潮大片在线观看 | 日韩v亚洲v欧美v精品综合 | 国产高潮流白浆免费视频 | 人妻有码av中文字幕久久琪 | 欧美色综合一区二区三区 | 精品人伦一区二区三区蜜桃免费 | 亚洲永久精品在线观看 |